I think it comes down to expansion rates of the plaster vs. Durabond. Everything in the home moves based on humidity and temp. If movement is not uniform, it can break the plane.

It will shrink a little as moisture evaporates, but is minimal compared to AP. I use DB for base coats, then finish AP.
 