As my local paint supplier started carrying Envirolak products, I want to start a thread on this line as there is a bit of a learning curve. First off, who here is using any of these products and which ones are you using? 1k, 2k, crosslinker? I've experimented a bit with some of it and it is next level, but as a finisher, changing between products is sometimes a gamble with cross contamination etc. What are you spraying the products with? How are you cleaning your machine between primers, different products etc..? My biggest concern right now, is that I'm trying to keep my system 1k, but if going to a deep base colour , you have to use 2 different primers. First is a White bonding primer(t9000) 2nd is a tintable(deep base) primer, so the top coat will stick. Has anyone found a way around this scenario.?(besides adding hardener) Having to prime twice is a pain and I just don't want to be spraying with isocyanates.